Hexcel® HexWeb® HRH-10/OX - 3/16 - 4.0 Aramid Fiber/Phenolic Resin Honeycomb

Category Other Engineering Material , Composite Core Material , Composite Fibers , Polymer , Thermoset , Aramid , Phenolic
Manufacturer Hexcel
Trade Name HexWeb®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® HRH-10/OX - 3/16 - 4.0 Aramid Fiber/Phenolic Resin Honeycomb.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the hexagonal or OX-Core confiation, the block is dipped in phenolic resin. After curing the resin, slices are cut to the desired thickness. For special applications, such as air directionalizing, HexWeb HRH-10 can be provided without the phenolic resin. Using this process, a wide range of cell sizes, paper thicknesses, and densities can be produced.Information provided by HexCel
Physical Properties Metric English Comments
Density 0.0641 g/cc
0.00231 lb/in³
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 3.45 MPa
>= 500 psi
Bare, min
>= 3.79 MPa
>= 550 psi
Stabilized, min
4.14 MPa
600 psi
Bare, typ
4.48 MPa
650 psi
Stabilized, typ
Compressive Modulus 0.179 GPa
26.0 ksi
Stabilized, typ
Shear Modulus 0.0317 GPa
4.60 ksi
Plate Shear, L Direction, typ
0.0579 GPa
8.40 ksi
Plate Shear, W Direction, typ
Shear Strength >= 0.724 MPa
>= 105 psi
Plate Shear, L Direction, min
>= 0.896 MPa
>= 130 psi
Plate Shear, W Direction, min
0.896 MPa
130 psi
Plate Shear, L Direction, typ
1.03 MPa
150 psi
Plate Shear, W Direction, typ