MS35J 120 24" EH04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2600 MPa
377000 psi
Tensile Modulus 183 GPa
26500 ksi
Flexural Yield Strength 1570 MPa
228000 psi
Flexural Modulus 205 GPa
29700 ksi
Compressive Yield Strength 1510 MPa
219000 psi
Compressive Modulus 164 GPa
23800 ksi
Shear Strength 84.1 MPa
12200 psi
Short Beam