Hexcel® HexForce™ SA120 Fiber Glass Fabric

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Hexcel
Trade Name HexForce™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexForce™ SA120 Fiber Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential allowing the end user to choose the best combination for material performance, economics and product flexibility.Information provided by Hexcel
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 12.2
Dry
Nominal Construction (count/in) 16
Warp
4
Fill
Type of Yarn Fill Yarn: Proprietary Heatset
Warp Yarn: SCG 750 Roving 463
Weave Style Plain Heatset