MV Labs CS300 Cs2CO3 Cesium carbonate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CS300 Cs2CO3 Cesium carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 325.82 g/mol
325.82 g/mol
Descriptive Properties Value Comments
Assay 81% Cs
CAS Number 534-17-8
Form White powder
Purity 99.995%
Typical Impurities Ba = 9; K = 2; Na, Rb, Sr = 1 ppm; Ca, Cr, Fe, Li, Mg, Mn, Si < 1 ND