Henkel Hysol EA 9689 Film Adhesive

Category Polymer , Adhesive , Film , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Henkel Hysol EA 9689 Film Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Modified epoxy film adhesive with high temperature strength and long-term thermal durability. Data from 0.10 psf, 500 g/m2.Applications: Composite Bonding Metal and Honeycomb Bonding
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 5.90 MPa
856 psi
Flatwise
Adhesive Bond Strength 22.0 MPa

@Temperature 177 °C
3190 psi

@Temperature 351 °F
Lap Shear
24.1 MPa

@Temperature 25.0 °C
3500 psi

@Temperature 77.0 °F
Lap Shear
25.5 MPa

@Temperature -55.0 °C
3700 psi

@Temperature -67.0 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 216 °C
421 °F
Glass Transition Temp, Tg 174 °C
345 °F
wet
224 °C
435 °F
dry
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 177 °C
1.00 hour

@Temperature 351 °F
Descriptive Properties Value Comments
Honeycomb Climbing Drum Peel, mN/m 35
at 25°C
Out-Time (days) 10
at 25°C