Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hardwire 3SX-12-12 Medium Density Composite

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel , Metal Foam, Mesh, or Honeycomb
Manufacturer Hardwire, LLC
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Hardwire 3SX-12-12 Medium Density Composite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The 3SX Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3SX cord is used where balanced compressive and tensile strengths are required as well as better handling characteristics than the 3S. The 3SX wire cord is made by twisting three identical wire filaments together (All filaments are 0.0189 in diameter) at a longer than usual lay length and then over-wrapping the bundle with a single filament. The result is a cord with lower twist angles and straighter filaments that is the basis for the increased compressive strengths.Characteristics: 3SX tapes have the highest compressive strengths of all Hardwire tapes and tend to match or exceed the tensile properties. Increased mechanical bonding in resins. Better interlaminar shear resistance. The cords do not bloom in failure modes during compression or tension. Laminates exhibit steel like characteristics with high ductility and extreme deflection capability. Very high flexural strength as well as ductile failure modes (laminates tend to bend – not break). The best tape for bending angles and can be done in standard sheet metal breaks. Very boardy feel – excellent for flat surfaces but still conformable enough for curved structures.Better handling characteristics and cutability than 3S tapes.All information provided by Hardwire, LLC.
Physical Properties Metric English Comments
Density 2.40 g/cc
0.0866 lb/in³
Laminate Density
Mechanical Properties Metric English Comments
Modulus of Elasticity 42.7 GPa
6200 ksi
Effective Modulus
Flexural Yield Strength 483 MPa
70000 psi
Sheet Stress
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved