H.C. Starck Standard 250 Titanium Carbide, TiC

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Standard 250 Titanium Carbide, TiC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC)
Physical Properties Metric English Comments
Particle Size 2.0 - 3.0 µm
2.0 - 3.0 µm
Average
4.5 - 7.0 µm
4.5 - 7.0 µm
Laser Diffraction D50
Component Elements Properties Metric English Comments
Carbon, C >= 19.2 %
>= 19.2 %
Free C <= 0.50 %
<= 0.50 %