H.C. Starck 2603 Molybdenum Powder Metallurgy Alloy ODS Mo-La

Category Metal , Nonferrous Metal , Molybdenum Alloy , Refractory Metal
Manufacturer H.C. Starck
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck 2603 Molybdenum Powder Metallurgy Alloy ODS Mo-La.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Powder Metallurgy Plate 2603Description of Product: This specification covers rolled, oxide-dispersion strengthened (ODS) molybdenum alloy (molybdenum + 2 vol% La2/O3) sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress relieved condition unless otherwise requested.Information provided by H.C. Starck.
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.0020 %
<= 0.0020 %
Calcium, Ca <= 0.0030 %
<= 0.0030 %
Carbon, C <= 0.0050 %
<= 0.0050 %
Chromium, Cr <= 0.010 %
<= 0.010 %
Copper, Cu <= 0.0020 %
<= 0.0020 %
Iron, Fe <= 0.010 %
<= 0.010 %
Lanthanum, La 1.0 - 1.2 %
1.0 - 1.2 %
Lead, Pb <= 0.0020 %
<= 0.0020 %
Magnesium, Mg <= 0.0010 %
<= 0.0010 %
Manganese, Mn <= 0.0010 %
<= 0.0010 %
Molybdenum, Mo >= 98.7 %
>= 98.7 %
by difference
Nickel, Ni <= 0.0050 %
<= 0.0050 %
Oxygen, O <= 0.25 %
<= 0.25 %
Silicon, Si <= 0.0050 %
<= 0.0050 %
Tin, Sn <= 0.0030 %
<= 0.0030 %
Titanium, Ti <= 0.0020 %
<= 0.0020 %