| Category | Ceramic , Oxide , Aluminum Oxide |
| Manufacturer | GBC Materials |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | GBC Grade 85 Alumina.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.40 g/cc | 0.123 lb/in³ | |
| Open Porosity | 0.00 % | 0.00 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Mohs | 9.0 | 9.0 | |
| Tensile Strength, Ultimate | 120 MPa | 17400 psi | |
| Flexural Strength | 310 MPa | 45000 psi | |
| Compressive Strength | 1700 MPa | 247000 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 6.70 µm/m-°C @Temperature 20.0 °C |
3.72 µin/in-°F @Temperature 68.0 °F |
|
| Maximum Service Temperature, Air | 1350 °C | 2460 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 85 % | 85 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 2.00e+10 ohm-cm | 2.00e+10 ohm-cm | |
| Dielectric Constant | 7.6 | 7.6 | |
| Dissipation Factor | 0.00060 | 0.00060 | |
| Dielectric Loss Index | 0.0060 | 0.0060 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | White |