Freudenberg Simrit S314 Silicone Elastomer (VMQ)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Freudenberg Simrit
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Freudenberg Simrit S314 Silicone Elastomer (VMQ).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasoline and solvents; poor resistance to alkalis and acids.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
Original Properties; ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
Original Properties; ASTM D2240
56

@Temperature 225 °C
56

@Temperature 437 °F
Air Aging, 70 hours; ASTM D2240
Tensile Strength, Ultimate 8.874 MPa
1287 psi
Original Properties; ASTM D412 Die C
6.5664 MPa

@Temperature 225 °C
952.38 psi

@Temperature 437 °F
Air Aging, 70 hours; ASTM D412 Die C
Elongation at Break 556 %
556 %
Original Properties; ASTM D412 Die C
300.24 %

@Temperature 225 °C
300.24 %

@Temperature 437 °F
Air Aging, 70 hours; ASTM D412 Die C
Tear Strength 27.7 kN/m
158 pli
ASTM D624 Die B
Compression Set 16 %

@Temperature 100 °C,
Time 79200 sec
16 %

@Temperature 212 °F,
Time 22.0 hour
ASTM D395
22 %

@Temperature 150 °C,
Time 252000 sec
22 %

@Temperature 302 °F,
Time 70.0 hour
ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -110 °C
-166 °F
ASTM D2137
Descriptive Properties Value Comments
Color Red
Low Temperature Brittleness Pass, No crack
ASTM D2137