Fainplast Compounds Propylplus 703 Polypropylene Cable Compound

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Fainplast Compounds
Trade Name Propylplus
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds Propylplus 703 Polypropylene Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polypropylene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid Polypropylene (flexible)Information provided by Fainplast Compounds
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 49
49
ISO 868
Tensile Strength at Break 25.0 MPa
3630 psi
50 mm/min; ISO 527
Elongation at Break 700 %
700 %
50 mm/min; ISO 527
Thermal Properties Metric English Comments
Vicat Softening Point 104 °C
219 °F
10N; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 2.26

@Frequency 1.00e+6 Hz
2.26

@Frequency 1.00e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 180 - 240 °C
356 - 464 °F