Transparent sheath, UL 94 Class V1
Physical Properties Metric English Comments
Density 1.18 - 1.22 g/cc
0.0426 - 0.0441 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 74
70 - 74
ISO R 868
Tensile Strength at Break 17.0 MPa
2470 psi
ISO R 527
Elongation at Break 260 %
260 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
Cold Flex; ISO 458/2
Flammability, UL94 V-1
V-1
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified