ExxonMobil Vistalon™ 404 Ethylene Propylene Copolymer Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Exxon Chemical
Trade Name Vistalon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Vistalon™ 404 Ethylene Propylene Copolymer Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Vistalon 404 rubber is a low Mooney, low ethylene copolymer with a broad molecular weight distribution. It is applicable for use in formulations for molded and mechanical goods. This product is sold in dense bales.Key Features: Easy processing and mixing.Information provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Mooney Viscosity 28

@Temperature 125 °C
28

@Temperature 257 °F
ML(1+4), Radial cavity dies, polymer remassed at 145±°C; ASTM D1646
Descriptive Properties Value Comments
Ethylene Content 45.0 wt%
ASTM D3900