ExxonMobil Santoprene® 8221-65M300 Thermoplastic Vulcanizate - UV Resistant

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8221-65M300 Thermoplastic Vulcanizate - UV Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good appearance. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable..Key Features: Neutral, easy coloring formulation.Excellent ozone resistance.Used in sealing applications.Recommended for applications requiring excellent flex fatigue resistance.EU and China RoHS compliant.Applications: Automotive – grips, Interior and Interior MatUses: Automotive ApplicationsAutomoitve Interior PartsOutdoor ApplicationsProcessing Method: Injection Moding and Multi Injection Molding Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 65

@Time 15.0 sec
65

@Time 0.00417 hour
2 mm; ISO 868
Tensile Strength at Break 4.70 MPa
682 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 420 %
420 %
Across Flow; ASTM D412 and ISO 37
Thermal Properties Metric English Comments
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 3 hour
3 hour