Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 181-57W180 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 181-57W180 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It has USP Class VI Certificate of Compliance for biocompatibility, MEM elution cytotoxicity to L-929 mouse fibroblast cells, 72 hour exposure to rubber extracts and USP physiochemical test for elastomer closures, heavy metals such as lead. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Key Features: Based on a series of biocompatibility tests conducted on representative grades, this grade should meet the USP (U.S. Pharmacopeia) Class VI requirements for plastics.Additionally some ISO 10993 tests have been conducted.Each medical grade undergoes annual testing for cytotoxicity and heavy metals.Drug master file maintained with the FDA.EU and China RoHS compliant.Applications:Medical – Soft Touch Grips, USP Class VI Seals and GasketsUses:Medical/Healthcare ApplicationsAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
2 mm, 15 sec; ISO 868
Tensile Strength at Break 4.67 MPa
677 psi
Across Flow; ASTM D412
Tensile Stress 2.00 MPa

@Strain 100 %
290 psi

@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 330 %
330 %
Across Flow; ASTM D412
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Color Black
Form Pellets