Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Compounding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, Exxon Chemical.23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It can also be used in coextrusions where adhesion and thermal processing stability are required or as an elastic, tough monolayer film.Applications: Compatibilizer and impact modifier for engineering thermoplastics; Coextruded tie layer for flexible packaging applications.
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
Exxon Method
Melt Flow 1.0 g/10 min
1.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Hardness, Shore D 33
33
ASTM D2240
Tensile Strength, Ultimate 11.0 MPa
1600 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0260 GPa
3.77 ksi
ASTM D790
Tensile Impact Strength 650 kJ/m²
309 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 74.0 °C
165 °F
Exxon Method
Vicat Softening Point 50.0 °C
122 °F
1000g; ASTM D-1525