Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Label-Lyte® 30 XU-001 Clear OPP High-shrink Film

Category Polymer , Adhesive , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte® 30 XU-001 Clear OPP High-shrink Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Clear, high-shrink film designed for use in roll-fed labeling of contoured containers such as aluminum and steel beverage cans, beaded metal cans, aerosol containers, and contoured glass and plastic bottles. It offers the high-shrink necessary for 202 beverage cans. This film is designed to laminate itself. The treated print surface is compatible with solvent-based or water-based flexo and gravure inks and UV-cured inks.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Thickness 30.5 microns
1.20 mil
Coating Weight >= 27.2 g/m²
>= 17.0 lb/ream
520
Thermal Properties Metric English Comments
Shrinkage, MD 26 %
26 %
at 275°F; 438
Shrinkage, TD 0.00 %
0.00 %
at 275°F; 438
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
444
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Wetting Tension, receding COS theta 40
Yield, in2/lb 25400