Physical Properties Metric English Comments
Thickness 30.5 microns
1.20 mil
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st..
Thickness 30.5 microns
1.20 mil
ExxonMobil Escorene® LL-1117 LLDPE Film/Sandwich Bag Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin. Films made from LL-1117 have very good tensile properties and toughness. This resin's good strength and drawability all..
Thickness 30.5 microns
1.20 mil
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert..
Thickness 30.5 microns
1.20 mil
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope..
Thickness 30.5 microns
1.20 mil
Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film  (discontinued **)
Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistanc..
Thickness 30.5 microns
1.20 mil
Nominal; ExxonMobil Method
ExxonMobil Bicor® 120 AB-X OPP Film
Product Description: Bicor AB-X is a two-side coated, sealable OPP film designed for general use in many applications, including overwrap, horizontal and vertical packaging. This film is suitable as..
Thickness 30.5 microns
1.20 mil
Nominal; ExxonMobil Method
ExxonMobil Bicor® 30 ARW OPP Film
Product Description: Bicor ARW is a two-side acrylic coated OPP film designed for use in lamination and monoweb applications, especially for paper ream wrap. The acrylic-coated side with the higher ..
Thickness 30.5 microns
1.20 mil
ExxonMobil Method
ExxonMobil Bicor™ 30MB666 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, ..
Thickness 30.5 microns
1.20 mil
ExxonMobil Method
ExxonMobil Bicor™ 30MBR666 OPP Film
Product Description: Bicor 30MBR is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high moist..
Thickness 30.5 microns
1.20 mil
ExxonMobil Hicor® 30 HF 104 OHD Film
One-side sealable, one-side treated, coextruded, oriented high density polyethylene film. It is ideal for use in HFFS and VFFS machines. It is designed to be used unsupported or in laminated applic..
Thickness 30.5 microns
1.20 mil
ExxonMobil Method
ExxonMobil Label-Lyte® 30 LLG-101 Clear OPP Film
Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (at other gauges of LLG-101) or applied ..
Thickness 30.5 microns
1.20 mil
ExxonMobil Label-Lyte® 30 XU-001 Clear OPP High-shrink Film
Clear, high-shrink film designed for use in roll-fed labeling of contoured containers such as aluminum and steel beverage cans, beaded metal cans, aerosol containers, and contoured glass and plastic..
Thickness 30.5 microns
1.20 mil
ExxonMobil Method
ExxonMobil Label-Lyte™ 30LL-101 OPP Film
Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as overlaminates in pressure-sensitive labeling appl..
Thickness 30.5 microns
1.20 mil
ExxonMobil Method
ExxonMobil Label-Lyte™ 30LL666 OPP Film
Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur..
Thickness 30.5 microns
1.20 mil
ExxonMobil Method
ExxonMobil Metallyte™ 30MM680 OPP Film
Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS ..
Thickness 30.5 microns
1.20 mil
ExxonMobil Method
ExxonMobil Oppalyte™ 30MW648 OPP Film
Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VTLS) coating. VLTS coating provides an excel..
Thickness 30.5 microns
1.20 mil
Nominal; ExxonMobil Method
ExxonMobil Bicor® 120 CSR-2 OPP Film
Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and ..
Thickness 30.5 microns
1.20 mil
Nominal; ExxonMobil Method
ExxonMobil Bicor® 120 LTSC OPP Film
Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS..
Thickness 30.5 microns
1.20 mil
ExxonMobil Method
ExxonMobil Bicor™ 30MBT666 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping, offering unique aspect and cost r..
Thickness 30.5 microns
1.20 mil
Backing; ASTM D3652
3M 5836 Clean-Walk Unframed Mat
3M™ Clean-Walk Unframed Mats 5830 Series are a multi-sheeted adhesive system that removes dirt and contaminates from shoe soles, wheels and other passing objects on contact. Comprised of a thin adh..
Thickness 30.5 microns
1.20 mil
Facestock
3M FP08R2 Clear Polypropylene Label Products
3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi..
Thickness 30.5 microns
1.20 mil
Backing; ASTM D3652
3M Scotch® 3721 Industrial Cold Temperature Box Sealing Tape
Scotch® Box Sealing Tape 3721 is an industrial cold temperature packaging tape for use at refrigeration temperatures, or at room temperature with subsequent storage at low temperatures. This produc..
Thickness 30.5 microns
1.20 mil
Backing; ASTM D3652
3M Scotch® 3779 Security Message Box Sealing Tape
Scotch® Security Message Box Sealing Tape 3779 is an industrial packaging tape used for box sealing specifically where security of the carton contents is a concern. The printed design along with th..
Thickness 30.5 microns
1.20 mil
Backing; ASTM D3652
3M 5850 Clean-View Pad
3M™ Clean-View Pad 5850 is an adhesive coated polyethylene film layered to form a pad of 20 removable sheets and designed for protection of windows and light fixtures from dirt and from chemical or..
Thickness 30.5 microns
1.20 mil
Backing; ASTM D3652
3M Scotch® 3781 Industrial Continuous Taping System Tape
Scotch® Taping System Tape 3781 is an industrial continuous packaging tape used for box sealing and specially designed for use with the 3M-Matic™ Continuous Taping System (CTS) stand. The Product ..
Thickness 30.5 microns
1.20 mil
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su..
Thickness 30.5 microns
1.20 mil
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope..
Thickness 30.5 microns
1.20 mil
Nominal
ExxonMobil Bicor® 120 LCX OPP Film
One-side treated, one-side sealable OPP film designed for use in a lamination. It is typically laminated to Metallyte, HBS-2, SPW, and itself to create lap sealable packages. The high energy surfac..
Thickness 30.5 microns
1.20 mil
ExxonMobil Method
ExxonMobil Oppalyte™ 30 HM-3 OPP Film
Product Description: A white opaque OPP film with a proprietary cavitated core. HM-3 is designed for cold seal applications and is used as a surface print, monoweb, or as the inside of lamination. I..
Thickness 30.5 microns
1.20 mil
ExxonMobil Method
ExxonMobil Oppalyte™ 30MW747 OPP Film
Product Description: White opaque biaxially oriented polypropylene film coated on one side acrylic, one side PVdC. Provides excellent performances on all packaging machines. 30MW747 is a super white..