Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Label-Lyte™ 150LL-302 OPP Film

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ExxonMobil Label-Lyte™ 150LL-302 OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A white, corona-treated polypropylene label facestock designed for rigid and semi-rigid pressure-sensitive applications requiring durability, opacity, and excellent graphic appeal. The treated, high energy, print surface has generally good compatibility with water-based and solvent-based flexo and gravure, UV flexo, UV letterpress, and UV screen ink systems. The print surface is also compatible with hot stamping systems. The adhesive side is corona-treated for good pressure-sensitive adhesive anchorage.Availability: Latin America, North America and South AmericaKey Features: High yield for excellent economicsCompatible with most major label printing technologiesTreated, high energy print surface for excellent ink adhesionExcellent opacity (for backside printing)Good stiffness for automatic and hand-applied label dispensingApplications:Dairy ProductsHealth and Beauty CareHousehold and DetergentsIndustrialPharmaceuticals Uses: Pressure Sensitive Labels Processing Method: Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, Thermal Transfer Printing and Water-based Flexographic PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Thickness 66.0 microns
2.60 mil
ExxonMobil Method
Coating Weight 46.1 g/m²
28.8 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 185 %
185 %
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 50 %
50 %
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, MD 90.3 MPa
13100 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 191 MPa
27700 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.3 %

@Temperature 135 °C
4.3 %

@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 5.0 %

@Temperature 135 °C
5.0 %

@Temperature 275 °F
ExxonMobil Method
Optical Properties Metric English Comments
Optical Density 2.3
2.3
ExxonMobil Method
Gloss 70 %
70 %
45°, Print Surface; ExxonMobil Method
Transmission, Visible 19 %
19 %
ExxonMobil Method
Descriptive Properties Value Comments
Opacity 0.88
Stiffness (Gurley) 22 mgf
MD
42 mgf
TD
Wetting Tension 0.85 receding cos theta
Adhesive Surface
0.9 receding cos theta
Print Surface
Yield 15000 in<sup>2</sup>/lb