ExxonMobil Escorene™ LD 706.15 Molding Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ExxonMobil Escorene™ LD 706.15 Molding Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for specialty molding, extrusion and compounding applications.Availability: Latin America, North America and South AmericaAdditive: Thermal Stabilizer: Yes Applications:Cap Seals and LinersCompoundingMasterbatch Base ResinInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
ExxonMobil method
Vinyl Acetate Content 14.9 %
14.9 %
ExxonMobil method
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 79

@Time 15.0 sec
79

@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 33

@Time 15.0 sec
33

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D638
Tensile Strength, Yield 5.31 MPa
770 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Elongation at Yield 130 %
130 %
ASTM D638
Flexural Modulus, 1% Secant 60.0 MPa
8700 psi
ASTM D790
Dart Drop, Total Energy 14.9 J

@Temperature 22.8 °C
11.0 ft-lb

@Temperature 73.0 °F
ASTM D3763
27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D3763
Thermal Properties Metric English Comments
Melting Point <= 190 °C
<= 374 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 61.1 °C
142 °F
ASTM D1525