Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ AD 0428EM1 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ AD 0428EM1 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: AD 0428EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: Yes Applications:Hot Melt AdhesivesInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ExxonMobil method
Vinyl Acetate Content 27.5 %
27.5 %
ExxonMobil method
Melt Flow 400 g/10 min
400 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.03 MPa
440 psi
ASTM D638
Elongation at Break 700 %
700 %
500 mm/min; ASTM D638
Tensile Modulus 0.0152 GPa
2.20 ksi
5.0 mm/min; ASTM D638
Thermal Properties Metric English Comments
Melting Point <= 160 °C
<= 320 °F
Peak Melting Point; ExxonMobil method
Users viewing this material also viewed the following: