ExxonMobil 32 Mobil EAL Envirosyn H Series

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil 32 Mobil EAL Envirosyn H Series.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems operating at moderate to severe conditions. They provide excellent wide temperature range performance above and beyond the capabilities of non-synthetic environmentally aware oils. Mobil EAL Envirosyn H Series provides exceptional anti-wear and film strength characteristics necessary for hydraulic systems operating under high load and high pressures. This is verified by their excellent wear control in the ASTM D 2882 and Vickers 35VQ25 Pump Wear Tests. Their 12-stage rating in the FZG Gear Load Test demonstrates a high level of protection against wear and scuffing and the suitability of this product to protect gears and bearings used in conjunction with hydraulic systems. The Mobil EAL Envirosyn H Seriess provide excellent protection against corrosion and ensures very good multi-metal compatibility allowing its use in systems employing various metallurgy that may be used in pump and component design. They also provide very good thin oil film protection against rusting. In addition to their exceptional performance capability, they satisfy the requirements for ready biodegradability and non-toxicity making them a desirable product for severe operating conditions where leakage or spillage of conventional oils could result in damage to the environment. Mobil EAL Envirosyn H Series oils are formulated from select, high-quality, high-VI synthetic base oil materials and high technology additive system specifically engineered to meet or exceed the performance requirements of most hydraulic pump and system builders while satisfying the stringent criteria for biodegradability and toxicity. Compared to the best vegetable oil-based and synthetic ester based hydraulic oils, these products provide improved oxidation stability and anti-foam performance, together with improved high and low temperature performance (-20º F to 200º F).Hydraulic systems where spills or leakage could result in damage to the environment; In systems where readily biodegradable and virtually non-toxic fluids may be required; Circulation systems containing gears and bearings where mild extreme-pressure characteristics are desired; Systems containing servo-valves; Hydraulic systems operating with oil temperatures in the range of -20F to 200F; Marine and mobile equipment operating in environmentally sensitive areas; Circulation systems operating under mild to moderate service conditions; Industrial hydraulic systems where leaked or spilled fluids could get into plant effluent; Air line oilers and some limited oil-mist generating systems; Air-over-hydraulic fluid systems operating in environmentally sensitive areas
Physical Properties Metric English Comments
Density 0.869 g/cc

@Temperature 15.0 °C
0.0314 lb/in³

@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 147
147
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 33.1 cSt
33.1 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 6.36 cSt
6.36 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -39.0 °C
-38.2 °F
ASTM D97
Flash Point 268 °C
514 °F
ASTM D92
Descriptive Properties Value Comments
Aquatic Toxicity, LC50, Trout, OECD 203, ppm 5000 (min)
Biodegradability, CO2 Conversion, % 60 (min)
EPA 560/6-82-003
FZG Gear Test, DIN 51534, Fail Stage 12
Rust Prevention, Synthetic Sea Water pass
ASTM D665B