Dow Corning 939 EMULSION

Category Fluid , Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 939 EMULSION.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW CORNING® 939 Cationic Emulsion is a 35 percent cationic emulsion of an amine-functional silicone polymer. The amodimethicone active is delivered in an opaque, low viscosity liquid with a neutral pH. It contains a non-tallow derived quaternary-amine surfactant and a biodegradable non-ionic surfactant. This emulsion enhances the conditioning performance of shampoos, conditioners and styling aids. The product provides easy formulation and good dilution stability.Information provided by Dow Corning
Physical Properties Metric English Comments
pH 7.6
7.6
Viscosity Measure 2000 cSt
2000 cSt
internal phase
Descriptive Properties Value Comments
Active Content (%) 35
Cationic yes
Solvent water