Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ex-Tech Plastics PerformaTech™ PVC Ex-Alloy 200 Reprocessed Vinyl

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Ex-Tech Plastics
Trade Name PerformaTech™ PVC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ex-Tech Plastics PerformaTech™ PVC Ex-Alloy 200 Reprocessed Vinyl.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ex-Tech Plastics has long been a market leader in reprocessing vinyl sheet used for a variety of high quality thermoformed packaging. From retail packaging to tri-folds to trays to blister and clamshell packaging. Characteristics: Superior utility grade Clear, standard and custom colors Tear resistantEnd Uses:Retail packagingBlister packagingClamshellsTri-foldsTraysInformation provided by Ex-Tech Plastics Inc.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 46.2 MPa
6700 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Modulus of Elasticity 2.07 GPa
300 ksi
ASTM D638
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
SOP-MEC-002.01
Thermal Properties Metric English Comments
Heat Distortion Temperature 62.0 °C
144 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 85 %
85 %
Gardner 20°
Descriptive Properties Value Comments
Appearance Blue Tint
Cold Impact -35°C
ASTM D1790
Users viewing this material also viewed the following: