Material Notes:
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.180 - 0.220 g/cc
0.00650 - 0.00795 lb/in³
ISO 845-88
Water Absorption <= 5.0 %
<= 5.0 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 60 - 70
60 - 70
ASTM D 2240
Tensile Strength 0.600 MPa
87.0 psi
ASTM D 412
Elongation at Break >= 150 %
>= 150 %
ASTM D 412
Compressive Yield Strength 0.0650 MPa

@Strain 25.0 %
9.43 psi

@Strain 25.0 %
ASTM 1056/85
0.120 MPa

@Strain 50.0 %
17.4 psi

@Strain 50.0 %
ASTM 1056/85
Tear Strength 0.400 kN/m
2.28 pli
ASTM D 624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 95.0 °C
203 °F
ASTM D 3575
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
ASTM D 3575
Flammability, UL94 HB
HB
HBF
Shrinkage <= 5.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 5.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Descriptive Properties Value Comments
Cellular Structure Closed
Color Black
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Fire Resistance MV22 302
Pass
Vulcanization Peroxide