Information provided by Lyondell.
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
20/20°C
Density 0.989 g/cc

@Temperature 20.0 °C
0.0357 lb/in³

@Temperature 68.0 °F
Solubility in Water 100 %
100 %
20°C
Viscosity 4.5 cP

@Temperature 25.0 °C
4.5 cP

@Temperature 77.0 °F
Molecular Weight 134.17 g/mol
134.17 g/mol
Vapor Pressure 0.000160 bar

@Temperature 20.0 °C
0.120 torr

@Temperature 68.0 °F
Evaporation Loss 2.0 %
2.0 %
n-BuAc=100%
Surface Tension 32.2 dynes/cm
32.2 dynes/cm
25°C
Thermal Properties Metric English Comments
Boiling Point 198 °C
388 °F
at 760 mmHg
Flash Point 91.0 °C
196 °F
Tag Closed Cup
Optical Properties Metric English Comments
Refractive Index 1.426

@Temperature 25.0 °C
1.426

@Temperature 77.0 °F
Descriptive Properties Value Comments