Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ASTM D792
Filler Content 45 %
45 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 104
104
ASTM D785
Tensile Strength 93.1 MPa
13500 psi
ASTM D638
Elongation at Break 1.9 %
1.9 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 9.65 GPa
1400 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 32.6 µm/m-°C
18.1 µin/in-°F
ASTM E831
Thermal Conductivity 0.0663 W/m-K
0.460 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 343 °C
649 °F
DSC
Descriptive Properties Value Comments
Color Black