Eifeler Coatings Technology EXXTRAL® rose PVD Coating

Category Ceramic , Nitride , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Eifeler Coatings Technology
Trade Name EXXTRAL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eifeler Coatings Technology EXXTRAL® rose PVD Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Characteristics: high hardness and elasticity, low friction, high oxidation resistancePrimary Applications: excellent for stainless steel and nickel-based high temperature alloys; hard and copy milling; interrupted cutting operations; lubricated, semi-dry or dry machiningInformation provided by Eifeler Coatings Technology
Physical Properties Metric English Comments
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Mechanical Properties Metric English Comments
Vickers Microhardness 2700 - 3300
2700 - 3300
Coefficient of Friction 0.20
0.20
dry, steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 800 °C
1470 °F
Descriptive Properties Value Comments
Color light rose