Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKASTER® F100 low-mid viscosity PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKASTER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKASTER® F100 low-mid viscosity PBT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical performance. Specially G/F reinforced PET has excellent heat resistance, a good surface, chemical resistance and high electrical performance.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
Linear Mold Shrinkage, Transverse 0.030 cm/cm
0.030 in/in
Mechanical Properties Metric English Comments
Tensile Strength 53.955 MPa
7825.5 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Strength 78.48 MPa
11380 psi
ASTM D790
Flexural Modulus 2.1582 GPa
313.02 ksi
ASTM D790
Izod Impact, Notched 0.343 J/cm
0.643 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
135 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 230 - 250 °C
446 - 482 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F