DuPont Teijin Films Teijin® Tetoron® HB3 Polyester Film, 200 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Teijin® Tetoron®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont Teijin Films Teijin® Tetoron® HB3 Polyester Film, 200 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Teijin® Tetoron® HB3 is a super smooth polyester film with a UV absorbing agent, originally designed for green house applications. It has excellent weather-durability, low color and low haze. It is pretreated on one side for slip and is available plain or knurled. Typical Applications: Greenhouse filmOpen air LabelsSolar Window FilmInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 160 %
160 %
ASTM D882A
Film Elongation at Break, TD 120 %
120 %
ASTM D882A
Coefficient of Friction, Dynamic 0.32
0.32
ASTM D1894
Coefficient of Friction, Static 0.31
0.31
ASTM D1894
Film Tensile Strength at Break, MD 224.94 MPa
32625 psi
ASTM D882A
Film Tensile Strength at Break, TD 244.94 MPa
35525 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 1.0 %

@Temperature 150 °C,
Time 1800 sec
1.0 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.20 %

@Temperature 150 °C,
Time 1800 sec
0.20 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 0.40 %
0.40 %
ASTM D1003