DuPont Teijin Films Mylar® EB31 Polyester Film, 200 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® EB31 Polyester Film, 200 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Mylar® EB31 is a smooth, matte polyester film. It does not contain any plasticizers. General Product Info: Mylar® EB31 has low haze and intermediate gloss. This offers more realistic colors and clearer text when reverse printing. Mylar® EB31 gives a bright appearance when metallized.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 102 %
102 %
ASTM D882A
Film Tensile Strength at Break, MD 138 MPa
20000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Shrinkage, MD 1.5 %

@Temperature 150 °C,
Time 1800 sec
1.5 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 60 %
60 %
ASTM D1003
Gloss 67 %
67 %
60°; ASTM D2457 - 90
Transmission, Visible 83 %
83 %
TLT; ASTM D1003