Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 359 Polyester Film, 700 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 359 Polyester Film, 700 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Melinex® 359 is a white opaque polyester film with a two side chemical pre-treatment for improved ink adhesion and laser printing.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 82.7 MPa
12000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 82.7 MPa
12000 psi
ASTM D882A
Coefficient of Friction, Dynamic 0.30 - 0.40
0.30 - 0.40
ASTM D1894
Film Tensile Strength at Break, MD 138 MPa
20000 psi
ASTM D882A
Film Tensile Strength at Break, TD 172 MPa
25000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 1.5 %

@Temperature 190 °C,
Time 300 sec
1.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.5 %

@Temperature 190 °C,
Time 300 sec
1.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Gloss 40 %
40 %
45°; ASTM D1003
45 %
45 %
60°; ASTM D1003
Transmission, Visible 6.5 %
6.5 %
TLT; ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 2889 in2/lb