Material Notes:
Surlyn® 8945 provides high flow properties and consistent, easy processing in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the ionomer spectrum.Surlyn® 8945 is ideal for applications where fast molding cycles at reduced molding temperatures are desired. The high flow characteristics also facilitate molding in thin sections. Surlyn® 8945 provides good cut resistance and high resiliency, particularly when used in blends with different cations, such as with surly® 9945.Information provided by DuPont.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Melt Index of Compound 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength at Break 22.1 MPa
3210 psi
ASTM D638
Tensile Strength, Yield 15.9 MPa
2310 psi
ASTM D638
Elongation at Break 330 %
330 %
ASTM D638
Flexural Modulus 0.448 GPa
65.0 ksi
ASTM D790(B)
Thermal Properties Metric English Comments
Melting Point 47.0 - 88.0 °C
117 - 190 °F
ASTM D3418(DSC)
Vicat Softening Point 71.0 °C
160 °F
ASTM D1525