| Category | Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® HTN |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Zytel® HTN 52G45HSL NC010 Polyphthalamide (PPA).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.56 g/cc | 0.0564 lb/in³ | DAM; ISO 1183 |
| Filler Content | 45 % | 45 % | DAM |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
DAM; ISO 527 |
| Tensile Stress | 11.26 MPa @Strain 0.100 %, Temperature 150 °C |
1633 psi @Strain 0.100 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
| 11.39 MPa @Strain 0.100 %, Temperature 100 °C |
1652 psi @Strain 0.100 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 13.35 MPa @Strain 0.100 %, Temperature -40.0 °C |
1936 psi @Strain 0.100 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 13.87 MPa @Strain 0.100 %, Temperature 23.0 °C |
2012 psi @Strain 0.100 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 | |
| 19.7 MPa @Strain 0.200 %, Temperature 150 °C |
2860 psi @Strain 0.200 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 22.49 MPa @Strain 0.200 %, Temperature 100 °C |
3262 psi @Strain 0.200 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 26.35 MPa @Strain 0.200 %, Temperature -40.0 °C |
3822 psi @Strain 0.200 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 26.68 MPa @Strain 0.300 %, Temperature 150 °C |
3870 psi @Strain 0.300 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 27.44 MPa @Strain 0.200 %, Temperature 23.0 °C |
3980 psi @Strain 0.200 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 | |
| 31.83 MPa @Strain 0.400 %, Temperature 150 °C |
4617 psi @Strain 0.400 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 32.1 MPa @Strain 0.300 %, Temperature 100 °C |
4660 psi @Strain 0.300 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 38.68 MPa @Strain 0.500 %, Temperature 150 °C |
5610 psi @Strain 0.500 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 39.23 MPa @Strain 0.400 %, Temperature 100 °C |
5690 psi @Strain 0.400 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 39.5 MPa @Strain 0.300 %, Temperature -40.0 °C |
5730 psi @Strain 0.300 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 40.65 MPa @Strain 0.300 %, Temperature 23.0 °C |
5896 psi @Strain 0.300 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 | |
| 43.1 MPa @Strain 0.600 %, Temperature 150 °C |
6250 psi @Strain 0.600 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 47.66 MPa @Strain 0.700 %, Temperature 150 °C |
6913 psi @Strain 0.700 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 48.97 MPa @Strain 0.500 %, Temperature 100 °C |
7103 psi @Strain 0.500 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 51.26 MPa @Strain 0.400 %, Temperature -40.0 °C |
7435 psi @Strain 0.400 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 51.57 MPa @Strain 0.800 %, Temperature 150 °C |
7480 psi @Strain 0.800 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 52.74 MPa @Strain 0.400 %, Temperature 23.0 °C |
7649 psi @Strain 0.400 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 | |
| 55.16 MPa @Strain 0.900 %, Temperature 150 °C |
8000 psi @Strain 0.900 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 56.14 MPa @Strain 0.600 %, Temperature 100 °C |
8142 psi @Strain 0.600 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 58.51 MPa @Strain 1.00 %, Temperature 150 °C |
8486 psi @Strain 1.00 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 61.76 MPa @Strain 1.10 %, Temperature 150 °C |
8958 psi @Strain 1.10 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 62.92 MPa @Strain 0.700 %, Temperature 100 °C |
9126 psi @Strain 0.700 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 64.75 MPa @Strain 1.20 %, Temperature 150 °C |
9391 psi @Strain 1.20 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 67.52 MPa @Strain 1.30 %, Temperature 150 °C |
9793 psi @Strain 1.30 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 68.05 MPa @Strain 0.500 %, Temperature -40.0 °C |
9870 psi @Strain 0.500 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 69.09 MPa @Strain 0.800 %, Temperature 100 °C |
10020 psi @Strain 0.800 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 69.39 MPa @Strain 0.500 %, Temperature 23.0 °C |
10060 psi @Strain 0.500 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 | |
| 70.11 MPa @Strain 1.40 %, Temperature 150 °C |
10170 psi @Strain 1.40 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 72.55 MPa @Strain 1.50 %, Temperature 150 °C |
10520 psi @Strain 1.50 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 74.58 MPa @Strain 0.900 %, Temperature 100 °C |
10820 psi @Strain 0.900 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 74.88 MPa @Strain 1.60 %, Temperature 150 °C |
10860 psi @Strain 1.60 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 76.99 MPa @Strain 1.70 %, Temperature 150 °C |
11170 psi @Strain 1.70 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 78.99 MPa @Strain 1.80 %, Temperature 150 °C |
11460 psi @Strain 1.80 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 79.57 MPa @Strain 1.00 %, Temperature 100 °C |
11540 psi @Strain 1.00 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 80.87 MPa @Strain 1.90 %, Temperature 150 °C |
11730 psi @Strain 1.90 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 82.63 MPa @Strain 2.00 %, Temperature 150 °C |
11980 psi @Strain 2.00 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 83.18 MPa @Strain 0.600 %, Temperature -40.0 °C |
12060 psi @Strain 0.600 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 83.56 MPa @Strain 0.600 %, Temperature 23.0 °C |
12120 psi @Strain 0.600 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 | |
| 84.26 MPa @Strain 2.10 %, Temperature 150 °C |
12220 psi @Strain 2.10 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 84.27 MPa @Strain 1.10 %, Temperature 100 °C |
12220 psi @Strain 1.10 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 85.77 MPa @Strain 2.20 %, Temperature 150 °C |
12440 psi @Strain 2.20 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 87.21 MPa @Strain 2.30 %, Temperature 150 °C |
12650 psi @Strain 2.30 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 88.55 MPa @Strain 2.40 %, Temperature 150 °C |
12840 psi @Strain 2.40 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 88.63 MPa @Strain 1.20 %, Temperature 100 °C |
12850 psi @Strain 1.20 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 89.77 MPa @Strain 2.50 %, Temperature 150 °C |
13020 psi @Strain 2.50 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 90.92 MPa @Strain 2.60 %, Temperature 150 °C |
13190 psi @Strain 2.60 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 91.99 MPa @Strain 2.70 %, Temperature 150 °C |
13340 psi @Strain 2.70 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 92.88 MPa @Strain 1.30 %, Temperature 100 °C |
13470 psi @Strain 1.30 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 93.01 MPa @Strain 2.80 %, Temperature 150 °C |
13490 psi @Strain 2.80 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 93.92 MPa @Strain 0.900 %, Temperature 150 °C |
13620 psi @Strain 0.900 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 94.71 MPa @Strain 3.00 %, Temperature 150 °C |
13740 psi @Strain 3.00 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 96.69 MPa @Strain 1.40 %, Temperature 100 °C |
14020 psi @Strain 1.40 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 97.41 MPa @Strain 0.700 %, Temperature 23.0 °C |
14130 psi @Strain 0.700 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 | |
| 98.06 MPa @Strain 0.700 %, Temperature -40.0 °C |
14220 psi @Strain 0.700 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 100.31 MPa @Strain 1.50 %, Temperature 100 °C |
14549 psi @Strain 1.50 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 103.72 MPa @Strain 1.60 %, Temperature 100 °C |
15043 psi @Strain 1.60 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 | |
| 106.56 MPa @Strain 1.70 %, Temperature 100 °C |
15455 psi @Strain 1.70 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 |