Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers VTR 8525 (GBLT-S) GLT 505 Formulation  (discontinued **)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers VTR 8525 (GBLT-S) GLT 505 Formulation  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FormulationViton® GLT 505
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Ultimate 16.5 MPa
2390 psi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Elongation at Break 190 %
190 %
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Modulus of Elasticity 0.000920 GPa
0.133 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
100% Modulus 0.00500 GPa
0.725 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Compression Set 17 %

@Temperature 200 °C
17 %

@Temperature 392 °F
Method B, O-rings 22 hr at 200°C (Post Cured 2 hr at 232°C)
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -30.8 °C
-23.4 °F
DSC