Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Hytrel® PC966 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer DuPont Performance Polymers
Trade Name Hytrel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® PC966 NC010 Polyester Elastomer TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
63 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D <= 63
<= 63
ISO 868
Tensile Strength at Break 43.0 MPa
6240 psi
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Charpy Impact, Notched 12.0 J/cm²
57.1 ft-lb/in²
Partial; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 210 °C
410 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >TPC-ET<
ISO 11469
Processing Coatable
Film Extrusion
Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification TPC-ET
ISO 1043
Special Characteristics High impact or impact modified
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved