Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Pro-faxâ„¢ SG722 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer LyondellBasell
Trade Name Pro-fax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-faxâ„¢ SG722 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Pro-faxâ„¢ SG722 high flow, high impact polypropylene copolymer resin is designed for injection molding applications. This resin is available in pellet form. Pro-faxâ„¢ SG722 resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520, for food contact, including cooking applications. All ingredients in Pro-faxâ„¢ SG722 resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Household goods, toys, consumer applications, sporting goodsInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.8 MPa
3300 psi
ASTM D 638
Elongation at Yield 6.6 %
6.6 %
ASTM D 638
Flexural Modulus 1.03 GPa
150 ksi
1% Secant, 0.05 in/min; ASTM D790
Izod Impact, Notched NB
NB
73°F; ASTM D256
Impact >= 45
>= 45
ft-lbs, Drop Weight Impact Strength, -29°C; Basell Test Method
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
Unannealed; ASTM D648
Optical Properties Metric English Comments
Gloss 86 %
86 %
Gardner, 60°; ASTM D523, tested in accordance with ASTM D2457
Users viewing this material also viewed the following: