Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792 - ISO 1183
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
ASTM D2240 - ISO 868
Tensile Strength at Break 5.20 MPa
754 psi
ASTM D638 - ISO 527-2
Elongation at Break 950 %
950 %
ASTM D638 - ISO 527-2
Thermal Properties Metric English Comments
Melting Point 72.0 °C
162 °F
ASTM D3418 - ISO 3146
Glass Transition Temp, Tg -55.0 °C
-67.0 °F
ASTM D3418