Dow Tyrin® CM0836 Chlorinated Polyethylene Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name Tyrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Tyrin® CM0836 Chlorinated Polyethylene Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: 36% chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible PVC in many uses. Can be calendered, injection molded, or extruded into tough, chemical and weather resistant products that can also provide built-in ignition resistance. Performance highlights include: inherent flexibility with plasticization; inherent chemical and ignition resistance; compatibility with PVC, PE, SAN, ABS, and other polymers, excellent low temperature properties, resistance to weathering, acceptance of fillers and heat/light stabilizers.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Volatiles <= 0.50 %
<= 0.50 %
100783-LE90A
Mooney Viscosity 94

@Temperature 121 °C
94

@Temperature 250 °F
ML 1 + 4; ASTM D1646
Descriptive Properties Value Comments
Chlorine Content 36 %
CPE D-6a