Dow Corning Z-6376 SILANE

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-6376 SILANE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Chloropropyltriethoxysilane - Used to pretreat or be added to the resin for integral treatment. Improves chemical bonding of resins to inorganic materials.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc

@Temperature 25.0 °C
1.01 g/cc

@Temperature 77.0 °F
Molecular Weight 240.5 g/mol
240.5 g/mol
Thermal Properties Metric English Comments
Boiling Point 223 °C
433 °F
Flash Point 61.0 °C
142 °F
closed cup
Descriptive Properties Value Comments
Active Content (%) 97