Unifrax Anchor-Loc®2 2600 Ceramic Fiber Modules

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Anchor-Loc®2 2600 Ceramic Fiber Modules.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Anchor-Loc®2 ceramic fiber modules extend the successful performance of standard Anchor-Loc folded modules to a product form featuring laminated fiber blanket constructin. This product combines advancements in fiber chemistry, manufacturing technology, and attachment hardware design to provide an economical lining system for a wide range of heat processing vessels.The Fibermass® manufacturing technique used to fabricate Anchor-Loc2 modules bonds layers of refractory ceramic fiber blanket into a strong pliable fiber block. Spun ceramic fiber blankets which feature high tensile strength for improved resistance to mechanical abuse, vibration, and gas velocity are used in the construction of Anchor-Loc2 Fibermass blocks. A proprietary fiber treatment decreases fiber dusting and irritation while increasing block flexibility, making the module easy to compress into place. Modules are available in two temperature grades based on construction from Durablanket® HP-S or Durablanket 2600.In all Anchor-Loc2 modules, Fibermass blocks are secured to the metallic module anchor with a pair of stainless steel support tubes. Flanges on one end of the support tubes effectively lock the position of the tubes relative to the anchor at the time of installation.Product AdvantagesFaster temperature cyclingLower heat storageLower fuel costsIncreased productivityLower installed costEasier repairsResistance to thermal shockApplicationsStress relievign furnacesAnnealing furnacesCar bottom heat treating furnacesProcess heatersReheat furnacesFurnace, kiln and boiler liningsIncineration equipment and stack liningsSoaking pit coversLadle coversLadle preheatersForge furnacesInformation Provided by Unifrax I LLC
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1343 °C
2449 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 29 - 31 %
29 - 31 %
SiO2 53 - 55 %
53 - 55 %
ZrO2 15 - 17 %
15 - 17 %
Descriptive Properties Value Comments
Temperature Grade (°C) 1427
Users viewing this material also viewed the following: