Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning HS II BASE & 10:1, COLORED CATALYST

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning HS II BASE & 10:1, COLORED CATALYST.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High strength silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items and better suited for thin section cure. HS II Base with HS II 10:1 Colored Catalyst is recommended for use with polyesters and plaster.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc

@Temperature 25.0 °C
1.21 g/cc

@Temperature 77.0 °F
Viscosity 20000 cP
20000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 16
16
Tensile Strength, Ultimate 3.79 MPa
550 psi
Elongation at Break 500 %
500 %
Tear Strength 22.8 kN/m
130 pli
Descriptive Properties Value Comments
Working Time (min) 90