Dow Corning 2-2677 Performance Modifier

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 2-2677 Performance Modifier.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity 1600 cP
1600 cP
Dynamic
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 100