Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Tensile Strength at Break 1.30 MPa
189 psi
Tensile stress at break.
Elongation at Break >= 1000 %
>= 1000 %
Secant Modulus 0.0177 GPa
2.57 ksi
2% Secant Modulus
Thermal Properties Metric English Comments
Vicat Softening Point 41.0 °C
106 °F