Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers Softflex® 8200

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Diamond and Network Polymers
Trade Name Softflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers Softflex® 8200.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 85
75 - 85
ASTM D2240
Tensile Strength, Yield 11.0 MPa
1600 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 800 %
800 %
chs 2.0 in/min; ASTM D638
Tear Strength 63.1 kN/m
360 pli
ASTM D624