| Category | Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Transparent |
| Manufacturer | Diamond and Network Polymers |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Diamond Polymers SAN 280 Styrene Acrylonitrile, Transparent Engineering Thermoplastic.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
| Melt Flow | 4.0 g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C |
4.0 g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F |
ASTM D1238 |
| 14.3 g/10 min <br>@Load 3.80 kg,<br> Temperature 230 °C |
14.3 g/10 min <br>@Load 8.38 lb,<br> Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 122 | 122 | ASTM D785 |
| Tensile Strength, Yield | 63.7 MPa | 9240 psi | chs 2.0 in/min; ASTM D638 |
| Flexural Modulus | 3.43 GPa | 497 ksi | chs 0.05 in/min; tangent; ASTM D790 |
| Izod Impact, Notched | 0.160 J/cm <br>@Thickness 3.17 mm,<br> Temperature 23.0 °C |
0.300 ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 106 °C <br>@Load 1.00 kg,<br> Thickness 3.17 mm |
223 °F <br>@Load 2.20 lb,<br> Thickness 0.125 in |
ASTM D1525 |
| Flammability, UL94 | HB <br>@Thickness 1.59 mm |
HB <br>@Thickness 0.0625 in |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 1.1 % | 1.1 % | ASTM D1003 |
| Transmission, Visible | 90.5 % | 90.5 % | ASTM D1003 |