Diamond Polymers NYLON 6001GF33 33% Glass Filled Polyamide

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NYLON 6001GF33 33% Glass Filled Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 157 MPa
22800 psi
ASTM D882
Elongation at Break 3.4 %
3.4 %
ASTM D882
Flexural Modulus 7.50 GPa
1090 ksi
ASTM D790
Izod Impact, Notched 0.980 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 227 °C
441 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 219 °C
426 °F
0.125";; ASTM D648