Crucible Steel 21-2N Martensitic Steel

Category Metal , Ferrous Metal , Austenitic , Stainless Steel
Manufacturer Crucible Steel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel 21-2N Martensitic Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Crucible Specialty Metals.
Mechanical Properties Metric English Comments
Hardness, Brinell <= 285
<= 285
Hardness, Rockwell C <= 42
<= 42
Tensile Strength, Ultimate >= 882.6 MPa
>= 128000 psi
Tensile Strength, Yield >= 490.3 MPa
>= 71110 psi
Elongation at Break >= 8.0 %
>= 8.0 %
Reduction of Area >= 5.0 %
>= 5.0 %
Component Elements Properties Metric English Comments
Carbon, C 0.50 - 0.60 %
0.50 - 0.60 %
Chromium, Cr 19.25 - 21.5 %
19.25 - 21.5 %
Iron, Fe >= 65 %
>= 65 %
As Remainder
Manganese, Mn 7.0 - 9.0 %
7.0 - 9.0 %
Nickel, Ni 1.5 - 2.75 %
1.5 - 2.75 %
Nitrogen, N 0.20 - 0.40 %
0.20 - 0.40 %
Silicon, Si <= 0.25 %
<= 0.25 %
Descriptive Properties Value Comments
Heat Treatment, °C 1100-1150 W.C.; 730-780 A.C.