| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant |
| Manufacturer | Covestro |
| Trade Name | Makrolon® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Covestro Makrolon® 2803 Polycarbonate, Injection Grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | |
| Water Absorption | 0.35 % | 0.35 % | Saturation in water |
| Moisture Absorption at Equilibrium | 0.15 % | 0.15 % | Equilibrium at 50% RH |
| Water Absorption at Saturation | 0.35 % | 0.35 % | |
| Melt Flow | 9.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 63.0 MPa | 9140 psi | |
| Elongation at Break | >= 50 % | >= 50 % | Nominal |
| Elongation at Yield | 6.0 % | 6.0 % | |
| Tensile Modulus | 2.40 GPa | 348 ksi | |
| Charpy Impact Unnotched | NB | NB | |
| Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | |
| Tensile Creep Modulus, 1000 hours | 1900 MPa | 276000 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 138 °C | 280 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 131 °C | 268 °F | |
| Vicat Softening Point | 147 °C | 297 °F | |
| Glass Transition Temp, Tg | 148 °C | 298 °F | |
| Flammability, UL94 | V-2 @Thickness 1.60 mm |
V-2 @Thickness 0.0630 in |
|
| V-2 @Thickness 2.40 mm |
V-2 @Thickness 0.0945 in |
||
| Oxygen Index | 26 % | 26 % |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.586 | 1.586 | DIN 5026-1 |
| Transmission, Visible | 88 % @Thickness 1.00 mm |
88 % @Thickness 0.0394 in |
ISO 489-A |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | |
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | |
| Dielectric Constant | 2.9 @Frequency 1e+6 Hz |
2.9 @Frequency 1e+6 Hz |
|
| 3.0 @Frequency 100 Hz |
3.0 @Frequency 100 Hz |
||
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
| Dissipation Factor | 0.0010 @Frequency 100 Hz |
0.0010 @Frequency 100 Hz |
|
| 0.010 @Frequency 1e+6 Hz |
0.010 @Frequency 1e+6 Hz |
||
| Comparative Tracking Index | 275 V | 275 V |