ConocoPhillips Syncon® 75W-90 HP Synthetic Gear Oil

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer ConocoPhillips
Trade Name Syncon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Syncon® 75W-90 HP Synthetic Gear Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Syncon HP Synthetic Gear Oil is recommended for conventional and limited-slip differentials, as well as some manual transmissions commonly found in passenger cars, race cars, trucks, vans, buses and offroad equipment operating in extreme temperatures or severe driving conditions. Syncon HP Synthetic Gear Oil is suited for top-off use in limited-slip differentials that normally require a friction modifier to prevent clutch chatter and slippage. This synthetic gear oil meets API GL-5 and MT-1 specifications and is approved under MIL-L-2105E. The SAE 75W-90 and 80W-140 grades are approved by Eaton Corp. as alternatives to Eaton Roadranger synthetic lubricants. To qualify for Eaton's seven-year/750,000-mile extended warranty using these products, consult a local Eaton representative. Syncon HP Synthetic Gear Oil is formulated with synthetic PAO base oils and selected additives to offer maximum protection against gear wear, rust and corrosion. It extends gear life and oil-drain intervals and reduces waste oil compared to conventional SAE 90, 80W-90 and 85W-140 gear oils. It is suited for high and low temperatures, offering thermal and oxidative stability and exceptional low-temperature fluidity.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
API Gravity 25.2 °
25.2 °
Viscosity Measurement 150
150
Viscosity Index
Saybolt Viscosity at 100°F 626 SUS
626 SUS
Saybolt Viscosity at 210°F 86 SUS
86 SUS
Kinematic Viscosity at 40°C (104°F) 137 cSt
137 cSt
Kinematic Viscosity at 100°C (212°F) 17 cSt
17 cSt
ASTM Color 6.5
6.5
Thermal Properties Metric English Comments
Pour Point -45.6 °C
-50.0 °F
Flash Point 207 °C
405 °F